| Item | ZGN-42 | GN-42 |
| Al2O3,% | ≥42 | ≥42 |
| Fe2O3,% | ≤1.6 | ≤1.7 |
| Refractoriness, ℃ | ≥1750 | ≥1750 |
| Appearance porosity,% | ≤15 | ≤16 |
| Cold crushing strength,MPa | ≥58.8 | ≥49.0 |
| Refractoriness under load,0.2Mpa,℃ | ≥1450 | ≥1430 |
| Linearing changes on reheating(1450℃×3h),% | 0~-0.2 | 0~-0.3 |